Synthesis and luminescence of SrAl2O4: Eu2+, Dy3+
Authors:
; Ahmad-Fauzi, M.; Nazarov, Michael V.; Azizan, A.; Azizan, A.
Summary:
This study systematically discusses the effects of the synthesis process of SrAl2O4:Eu2+, Dy3+ in reducing the firing temperature and reducing the percentage of concentration of Eu2O3 and Dy2O3. The influence of firing temperature and rare earth doping on crystal structure, morphology, and its luminescent properties were analyzed by X-ray diffraction (XRD), Raman scattering, Photoluminescence excitation (PLE) and photoluminescence emission (PL) spectroscopy, and scanning electron microscopy (SEM). The emission intensity becomes stronger as the firing temperature increases from 1100°C to 1250°C. SrAl2O4:Eu2+, Dy3+ firing at 1250°C shows the maximum photoluminescence intensity at 0.5 mol % Eu2O3 and 1 mol % Dy2O3 addition. A phase transformation from SrAl4O7 to SrAl2O4 and Sr4Al14O25 is found with increasing firing temperature. The synthesized phosphors reveal the presence of the crystalline monoclinic structure of SrAl2O4 as a major phase (JCPDS card no. 74-0794) and the intermediate phase orthorhombic structure of Sr4Al14O25. Small amount of doped Eu2O3 and Dy2O3 has almost no effect on the crystalline phase composition. The proposed firing temperature and mole concentration of the activator and co-activator is lower in comparison with other conventional solid state methods and allows us to obtain the SrAl2O4:Eu2+, Dy3+ phosphor with improved properties.
Export Metadata
Google Scholar
<meta name="citation_title" content="Synthesis and luminescence of SrAl2O4: Eu2+, Dy3+"> <meta name="citation_author" content=""> <meta name="citation_author" content="Ahmad-Fauzi, M."> <meta name="citation_author" content="Nazarov, Michael V."> <meta name="citation_author" content="Azizan, A."> <meta name="citation_author" content="Azizan, A."> <meta name="citation_publication_date" content="2012/01/03"> <meta name="citation_journal_title" content="Moldavian Journal of the Physical Sciences"> <meta name="citation_volume" content="11"> <meta name="citation_issue" content="1-2"> <meta name="citation_firstpage" content="78"> <meta name="citation_lastpage" content="93"> <meta name="citation_pdf_url" content="https://ibn.idsi.md/sites/default/files/imag_file/78-93_0.pdf">
Crossref
<?xml version='1.0' encoding='utf-8'?> <doi_batch version='4.3.7' xmlns='http://www.crossref.org/schema/4.3.7' xmlns:xsi='http://www.w3.org/2001/XMLSchema-instance' xsi:schemaLocation='http://www.crossref.org/schema/4.3.7 http://www.crossref.org/schema/deposit/crossref4.3.7.xsd'> <head> <doi_batch_id>ibn-18997</doi_batch_id> <timestamp>1597491218</timestamp> <depositor> <depositor_name>Information Society Development Instiute, Republic of Moldova</depositor_name> <email_address>mjps@nanotech.md</email_address> </depositor> <registrant>Institutul de Inginerie Electronică şi Nanotehnologii "D. Ghiţu" al AŞM</registrant> </head> <body> <journal> <journal_metadata> <full_title>Moldavian Journal of the Physical Sciences</full_title> <issn media_type='print'>1810648X</issn> </journal_metadata> <journal_issue> <publication_date media_type='print'> <year>2012</year> </publication_date> <issue>1-2(11)</issue> </journal_issue> <journal_article publication_type='full_text'><titles> <title>Synthesis and luminescence of SrAl2O4: Eu2+, Dy3+</title> </titles> <contributors> <person_name sequence='first' contributor_role='author'> <given_name>AwangNor</given_name> <surname>Nazida</surname> </person_name> <person_name sequence='additional' contributor_role='author'> <given_name>M.</given_name> <surname>Ahmad-Fauzi</surname> </person_name> <person_name sequence='additional' contributor_role='author'> <given_name>Mihail</given_name> <surname>Nazarov</surname> </person_name> <person_name sequence='additional' contributor_role='author'> <given_name>A.</given_name> <surname>Azizan</surname> </person_name> <person_name sequence='additional' contributor_role='author'> <given_name>K.</given_name> <surname>ShahRizal</surname> </person_name> </contributors> <publication_date media_type='print'> <year>2012</year> </publication_date> <pages> <first_page>78</first_page> <last_page>93</last_page> </pages> </journal_article> </journal> </body> </doi_batch>
CERIF
<?xml version='1.0' encoding='utf-8'?> <CERIF xmlns='urn:xmlns:org:eurocris:cerif-1.5-1' xsi:schemaLocation='urn:xmlns:org:eurocris:cerif-1.5-1 http://www.eurocris.org/Uploads/Web%20pages/CERIF-1.5/CERIF_1.5_1.xsd' xmlns:xsi='http://www.w3.org/2001/XMLSchema-instance' release='1.5' date='2012-10-07' sourceDatabase='Output Profile'> <cfResPubl> <cfResPublId>ibn-ResPubl-18997</cfResPublId> <cfResPublDate>2012-01-03</cfResPublDate> <cfVol>11</cfVol> <cfIssue>1-2</cfIssue> <cfStartPage>78</cfStartPage> <cfISSN>1810-648X</cfISSN> <cfURI>http://mjps.utm.md/archive/2012/article/18997</cfURI> <cfTitle cfLangCode='EN' cfTrans='o'>Synthesis and luminescence of SrAl2O4: Eu2+, Dy3+</cfTitle> <cfAbstr cfLangCode='EN' cfTrans='o'><p>This study systematically discusses the effects of the synthesis process of SrAl2O4:Eu2+, Dy3+ in reducing the firing temperature and reducing the percentage of concentration of Eu2O3 and Dy2O3. The influence of firing temperature and rare earth doping on crystal structure, morphology, and its luminescent properties were analyzed by X-ray diffraction (XRD), Raman scattering, Photoluminescence excitation (PLE) and photoluminescence emission (PL) spectroscopy, and scanning electron microscopy (SEM). The emission intensity becomes stronger as the firing temperature increases from 1100°C to 1250°C. SrAl2O4:Eu2+, Dy3+ firing at 1250°C shows the maximum photoluminescence intensity at 0.5 mol % Eu2O3 and 1 mol % Dy2O3 addition. A phase transformation from SrAl4O7 to SrAl2O4 and Sr4Al14O25 is found with increasing firing temperature. The synthesized phosphors reveal the presence of the crystalline monoclinic structure of SrAl2O4 as a major phase (JCPDS card no. 74-0794) and the intermediate phase orthorhombic structure of Sr4Al14O25. Small amount of doped Eu2O3 and Dy2O3 has almost no effect on the crystalline phase composition. The proposed firing temperature and mole concentration of the activator and co-activator is lower in comparison with other conventional solid state methods and allows us to obtain the SrAl2O4:Eu2+, Dy3+ phosphor with improved properties.</p></cfAbstr> <cfResPubl_Class> <cfClassId>eda2d9e9-34c5-11e1-b86c-0800200c9a66</cfClassId> <cfClassSchemeId>759af938-34ae-11e1-b86c-0800200c9a66</cfClassSchemeId> <cfStartDate>2012-01-03T24:00:00</cfStartDate> </cfResPubl_Class> <cfResPubl_Class> <cfClassId>e601872f-4b7e-4d88-929f-7df027b226c9</cfClassId> <cfClassSchemeId>40e90e2f-446d-460a-98e5-5dce57550c48</cfClassSchemeId> <cfStartDate>2012-01-03T24:00:00</cfStartDate> </cfResPubl_Class> <cfPers_ResPubl> <cfPersId>ibn-person-34468</cfPersId> <cfClassId>49815870-1cfe-11e1-8bc2-0800200c9a66</cfClassId> <cfClassSchemeId>b7135ad0-1d00-11e1-8bc2-0800200c9a66</cfClassSchemeId> <cfStartDate>2012-01-03T24:00:00</cfStartDate> </cfPers_ResPubl> <cfPers_ResPubl> <cfPersId>ibn-person-34488</cfPersId> <cfClassId>49815870-1cfe-11e1-8bc2-0800200c9a66</cfClassId> <cfClassSchemeId>b7135ad0-1d00-11e1-8bc2-0800200c9a66</cfClassSchemeId> <cfStartDate>2012-01-03T24:00:00</cfStartDate> </cfPers_ResPubl> <cfPers_ResPubl> <cfPersId>ibn-person-42324</cfPersId> <cfClassId>49815870-1cfe-11e1-8bc2-0800200c9a66</cfClassId> <cfClassSchemeId>b7135ad0-1d00-11e1-8bc2-0800200c9a66</cfClassSchemeId> <cfStartDate>2012-01-03T24:00:00</cfStartDate> </cfPers_ResPubl> <cfPers_ResPubl> <cfPersId>ibn-person-34489</cfPersId> <cfClassId>49815870-1cfe-11e1-8bc2-0800200c9a66</cfClassId> <cfClassSchemeId>b7135ad0-1d00-11e1-8bc2-0800200c9a66</cfClassSchemeId> <cfStartDate>2012-01-03T24:00:00</cfStartDate> </cfPers_ResPubl> <cfPers_ResPubl> <cfPersId>ibn-person-34490</cfPersId> <cfClassId>49815870-1cfe-11e1-8bc2-0800200c9a66</cfClassId> <cfClassSchemeId>b7135ad0-1d00-11e1-8bc2-0800200c9a66</cfClassSchemeId> <cfStartDate>2012-01-03T24:00:00</cfStartDate> </cfPers_ResPubl> </cfResPubl> <cfPers> <cfPersId>ibn-Pers-34468</cfPersId> <cfPersName_Pers> <cfPersNameId>ibn-PersName-34468-3</cfPersNameId> <cfClassId>55f90543-d631-42eb-8d47-d8d9266cbb26</cfClassId> <cfClassSchemeId>7375609d-cfa6-45ce-a803-75de69abe21f</cfClassSchemeId> <cfStartDate>2012-01-03T24:00:00</cfStartDate> </cfPersName_Pers> </cfPers> <cfPers> <cfPersId>ibn-Pers-34488</cfPersId> <cfPersName_Pers> <cfPersNameId>ibn-PersName-34488-3</cfPersNameId> <cfClassId>55f90543-d631-42eb-8d47-d8d9266cbb26</cfClassId> <cfClassSchemeId>7375609d-cfa6-45ce-a803-75de69abe21f</cfClassSchemeId> <cfStartDate>2012-01-03T24:00:00</cfStartDate> <cfFamilyNames>Ahmad-Fauzi</cfFamilyNames> <cfFirstNames>M.</cfFirstNames> </cfPersName_Pers> </cfPers> <cfPers> <cfPersId>ibn-Pers-42324</cfPersId> <cfPersName_Pers> <cfPersNameId>ibn-PersName-42324-3</cfPersNameId> <cfClassId>55f90543-d631-42eb-8d47-d8d9266cbb26</cfClassId> <cfClassSchemeId>7375609d-cfa6-45ce-a803-75de69abe21f</cfClassSchemeId> <cfStartDate>2012-01-03T24:00:00</cfStartDate> <cfFamilyNames>Nazarov</cfFamilyNames> <cfFirstNames>Michael V.</cfFirstNames> </cfPersName_Pers> </cfPers> <cfPers> <cfPersId>ibn-Pers-34489</cfPersId> <cfPersName_Pers> <cfPersNameId>ibn-PersName-34489-3</cfPersNameId> <cfClassId>55f90543-d631-42eb-8d47-d8d9266cbb26</cfClassId> <cfClassSchemeId>7375609d-cfa6-45ce-a803-75de69abe21f</cfClassSchemeId> <cfStartDate>2012-01-03T24:00:00</cfStartDate> <cfFamilyNames>Azizan</cfFamilyNames> <cfFirstNames>A.</cfFirstNames> </cfPersName_Pers> </cfPers> <cfPers> <cfPersId>ibn-Pers-34490</cfPersId> <cfPersName_Pers> <cfPersNameId>ibn-PersName-34490-3</cfPersNameId> <cfClassId>55f90543-d631-42eb-8d47-d8d9266cbb26</cfClassId> <cfClassSchemeId>7375609d-cfa6-45ce-a803-75de69abe21f</cfClassSchemeId> <cfStartDate>2012-01-03T24:00:00</cfStartDate> </cfPersName_Pers> </cfPers> </CERIF>
BibTeX
@article{ibn_18997,
author = {Ahmad-Fauzi, M.N. and Nazarov, M. and Azizan, A.},
title = {Synthesis and luminescence of SrAl2O4: Eu2+, Dy3+},
journal = {Moldavian Journal of the Physical Sciences},
year = {2012},
volume = {11 (1-2)},
pages = {78-93},
month = {Jan},
abstract = {(EN) <p>This study systematically discusses the effects of the synthesis process of SrAl2O4:Eu2+, Dy3+ in reducing the firing temperature and reducing the percentage of concentration of Eu2O3 and Dy2O3. The influence of firing temperature and rare earth doping on crystal structure, morphology, and its luminescent properties were analyzed by X-ray diffraction (XRD), Raman scattering, Photoluminescence excitation (PLE) and photoluminescence emission (PL) spectroscopy, and scanning electron microscopy (SEM). The emission intensity becomes stronger as the firing temperature increases from 1100°C to 1250°C. SrAl2O4:Eu2+, Dy3+ firing at 1250°C shows the maximum photoluminescence intensity at 0.5 mol % Eu2O3 and 1 mol % Dy2O3 addition. A phase transformation from SrAl4O7 to SrAl2O4 and Sr4Al14O25 is found with increasing firing temperature. The synthesized phosphors reveal the presence of the crystalline monoclinic structure of SrAl2O4 as a major phase (JCPDS card no. 74-0794) and the intermediate phase orthorhombic structure of Sr4Al14O25. Small amount of doped Eu2O3 and Dy2O3 has almost no effect on the crystalline phase composition. The proposed firing temperature and mole concentration of the activator and co-activator is lower in comparison with other conventional solid state methods and allows us to obtain the SrAl2O4:Eu2+, Dy3+ phosphor with improved properties.</p>},
url = {https://ibn.idsi.md/vizualizare_articol/18997},
}
DataCite
<?xml version='1.0' encoding='utf-8'?> <resource xmlns:xsi='http://www.w3.org/2001/XMLSchema-instance' xmlns='http://datacite.org/schema/kernel-3' xsi:schemaLocation='http://datacite.org/schema/kernel-3 http://schema.datacite.org/meta/kernel-3/metadata.xsd'> <creators> <creator> <creatorName></creatorName> <affiliation>School of Materials and Mineral Resources Engineering, University Sains Malaysia, Malaysia</affiliation> </creator> <creator> <creatorName>Ahmad-Fauzi, M.N.</creatorName> <affiliation>School of Materials and Mineral Resources Engineering, University Sains Malaysia, Malaysia</affiliation> </creator> <creator> <creatorName>Nazarov, M.</creatorName> <affiliation>Institutul de Fizică Aplicată al AŞM, Moldova, Republica</affiliation> </creator> <creator> <creatorName>Azizan, A.</creatorName> <affiliation>School of Materials and Mineral Resources Engineering, University Sains Malaysia, Malaysia</affiliation> </creator> <creator> <creatorName>Azizan, A.</creatorName> <affiliation>School of Materials and Mineral Resources Engineering, University Sains Malaysia, Malaysia</affiliation> </creator> </creators> <titles> <title xml:lang='en'>Synthesis and luminescence of SrAl2O4: Eu2+, Dy3+</title> </titles> <publisher>Instrumentul Bibliometric National</publisher> <publicationYear>2012</publicationYear> <relatedIdentifier relatedIdentifierType='ISSN' relationType='IsPartOf'>1810-648X</relatedIdentifier> <dates> <date dateType='Issued'>2012-01-03</date> </dates> <resourceType resourceTypeGeneral='Text'>Journal article</resourceType> <descriptions> <description xml:lang='en' descriptionType='Abstract'><p>This study systematically discusses the effects of the synthesis process of SrAl2O4:Eu2+, Dy3+ in reducing the firing temperature and reducing the percentage of concentration of Eu2O3 and Dy2O3. The influence of firing temperature and rare earth doping on crystal structure, morphology, and its luminescent properties were analyzed by X-ray diffraction (XRD), Raman scattering, Photoluminescence excitation (PLE) and photoluminescence emission (PL) spectroscopy, and scanning electron microscopy (SEM). The emission intensity becomes stronger as the firing temperature increases from 1100°C to 1250°C. SrAl2O4:Eu2+, Dy3+ firing at 1250°C shows the maximum photoluminescence intensity at 0.5 mol % Eu2O3 and 1 mol % Dy2O3 addition. A phase transformation from SrAl4O7 to SrAl2O4 and Sr4Al14O25 is found with increasing firing temperature. The synthesized phosphors reveal the presence of the crystalline monoclinic structure of SrAl2O4 as a major phase (JCPDS card no. 74-0794) and the intermediate phase orthorhombic structure of Sr4Al14O25. Small amount of doped Eu2O3 and Dy2O3 has almost no effect on the crystalline phase composition. The proposed firing temperature and mole concentration of the activator and co-activator is lower in comparison with other conventional solid state methods and allows us to obtain the SrAl2O4:Eu2+, Dy3+ phosphor with improved properties.</p></description> </descriptions> <formats> <format>application/pdf</format> </formats> </resource>
Dublin Core
<?xml version='1.0' encoding='utf-8'?> <oai_dc:dc xmlns:dc='http://purl.org/dc/elements/1.1/' xmlns:oai_dc='http://www.openarchives.org/OAI/2.0/oai_dc/' xmlns:xsi='http://www.w3.org/2001/XMLSchema-instance' xsi:schemaLocation='http://www.openarchives.org/OAI/2.0/oai_dc/ http://www.openarchives.org/OAI/2.0/oai_dc.xsd'> <dc:creator></dc:creator> <dc:creator>Ahmad-Fauzi, M.N.</dc:creator> <dc:creator>Nazarov, M.</dc:creator> <dc:creator>Azizan, A.</dc:creator> <dc:creator>Azizan, A.</dc:creator> <dc:date>2012-01-03</dc:date> <dc:description xml:lang='en'><p>This study systematically discusses the effects of the synthesis process of SrAl2O4:Eu2+, Dy3+ in reducing the firing temperature and reducing the percentage of concentration of Eu2O3 and Dy2O3. The influence of firing temperature and rare earth doping on crystal structure, morphology, and its luminescent properties were analyzed by X-ray diffraction (XRD), Raman scattering, Photoluminescence excitation (PLE) and photoluminescence emission (PL) spectroscopy, and scanning electron microscopy (SEM). The emission intensity becomes stronger as the firing temperature increases from 1100°C to 1250°C. SrAl2O4:Eu2+, Dy3+ firing at 1250°C shows the maximum photoluminescence intensity at 0.5 mol % Eu2O3 and 1 mol % Dy2O3 addition. A phase transformation from SrAl4O7 to SrAl2O4 and Sr4Al14O25 is found with increasing firing temperature. The synthesized phosphors reveal the presence of the crystalline monoclinic structure of SrAl2O4 as a major phase (JCPDS card no. 74-0794) and the intermediate phase orthorhombic structure of Sr4Al14O25. Small amount of doped Eu2O3 and Dy2O3 has almost no effect on the crystalline phase composition. The proposed firing temperature and mole concentration of the activator and co-activator is lower in comparison with other conventional solid state methods and allows us to obtain the SrAl2O4:Eu2+, Dy3+ phosphor with improved properties.</p></dc:description> <dc:source>Moldavian Journal of the Physical Sciences 11 (1-2) 78-93</dc:source> <dc:title>Synthesis and luminescence of SrAl2O4: Eu2+, Dy3+</dc:title> <dc:type>info:eu-repo/semantics/article</dc:type> </oai_dc:dc>